In terms of pump material and structure, if it is a non-corrosive liquid, carbon steel is used for pressure-resistant parts below 370°C, and 5% or 13% chromium steel is used above 370°C; for parts with low strength , cast iron can be used below 230 ℃. When the thermal expansion coefficients of th..